Scale out, corrosion checked
Two different failures, two different jobs. Flushing removes mineral — at 240 mg/L of calcium carbonate, scale settles on the tank floor and the burner heats it alongside the water, so capacity and recovery decline.
The anode rod addresses corrosion. It corrodes so the steel does not, and once spent the shell fails from the base upward, which is why a tank can look healthy and be near its end.
The visit
Drains and flushes until clear, inspects and replaces the anode where needed, tests the relief valve and confirms the discharge is clear, and reviews the pan, drain, strapping and venting. Power or gas only once the tank is full.
When not to spend
A tank leaking at the base is not a maintenance candidate, and a heavily scaled tank on a corroded floor can start leaking when the sediment is disturbed.